After the platform had run a pressure test, it had became apparent that a 3 mm hole had appeared at the 6 o’clock position of a weld on the 4″ CIP line.
4 Inch CIP Line Repair
After the platform had run a pressure test, it had became apparent that a 3 mm hole had appeared at the 6 o’clock position of a weld on the 4″ CIP line.
There was two areas at the front of the strainer that had severe internal corrosion.